Polymer Property : Film Tensile Strength at Break, TD = 15300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 105 MPa
15300 psi
ASTM D882
Dow Saran® 560 Vapor Retarder Film
Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 600 gauge. Roll size: 35.5" x 250 long.Informat..