Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 108 MPa | 15600 psi | ASTM D882A |
DuPont Teijin Films Melinex® CORE 2 Polyester Film Melinex® CORE 2 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well.. |