Polymer Property : Dart Drop Test = 96.0 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 96.0 g
0.212 lb
Method A; ASTM D1709
Dow 621I Low Density Polyethylene (LDPE)
Specialty resin designed for high melt strength applications Provides excellent bubble stability Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Dart Drop Test 96.0 g
0.212 lb
Method A; ASTM D1709
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed..