Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 85.0 g | 0.187 lb | ASTM D1709 |
SABIC 218 Series Linear Low Density Polyethylene for Blown Film Product Description: 218 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. They are easy to process giving good tensile properties, impact strength a.. |
|||
Dart Drop Test | 85.0 g | 0.187 lb | ASTM D1709 |
SABIC 726 Series Linear Low Density Polyethylene for Blown Film Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher .. |
|||
Dart Drop Test | 85.0 g | 0.187 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Dart Drop Test | 85.0 g | 0.187 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Dart Drop Test | 85.0 g | 0.187 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Dart Drop Test | 85.0 - 100 g | 0.187 - 0.221 lb | ASTM D1709 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Dart Drop Test | 85.0 - 700 g | 0.187 - 1.54 lb | Average value: 290 g Grade Count:5 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Dart Drop Test | 85.0 g | 0.187 lb | ASTM D1709 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |