Polymer Property : Dart Drop Test = 78.0 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 78.0 g
0.172 lb
ASTM D1709
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film
Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn..
Dart Drop Test 78.0 g
0.172 lb
Method A; ASTM D1709
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow