Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 65.0 g | 0.143 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D1709 |
Huntsman PE1080 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with high clarity and excellent stiffness.Applications: Film extrusion: overwrapFDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D1709 |
M. Holland Company LD225 LDPE
(discontinued **) Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, High Clarity, High Gloss, Heat Sealable, Good Processability, Medium SlipUses: FilmProcessing Method: Blown FilmInformation pro.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA334000 Low Density Polyethylene ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | Blown; ASTM D1709, F<sub>50</sub> |
LyondellBasell Petrothene® NA373244 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D1709 |
LG Chemical SEETEC BF410 LDPE Characteristics: Good Processability and Excellent Optical PropertiesAdditives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG .. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D1709 |
Iran Petrochemical (PCC) 16503 Linear Low Density Polyethylene 16503 is a LLDPE for general purpose cast stretch film grade. The ease of processing and the low gels make 16503 well suited for production of general purpose monolayer or multilayer cast stretch fi.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | Blown; ASTM D1709, F<sub>50</sub> |
LyondellBasell Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade ApplicationsPetrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D-1709 |
Bapolene® 222B Polyethylene Film Grade Bapolene 222B is a butene linear low density polyethylene for blown film applications requiring superior impact strength and toughness. It complies with US FDA 21CFR177.1520.Applications: General p.. |
|||
Dart Drop Test | 65.0 g | 0.143 lb | ASTM D 1709 A |
Total Lacqtene® 6002 FLG 42 HDPE film
(discontinued **) LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h.. |
|||
Dart Drop Test | 65.0 - 120 g | 0.143 - 0.265 lb | Average value: 95.0 g Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |