Polymer Property : Dart Drop Test = 560 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 560 g
1.23 lb
22; ASTM D 1709/A
NOVA Chemicals Sclair® FP019-C Octene Copolymer LLDPE Film Resin
FP019-C is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Polymer Process AidApplications: High toughness film,..
Dart Drop Test 560 g
1.23 lb
22; ASTM D 1709/A
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin
FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig..