Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 29.0 g | 0.0639 lb | F<sub>50</sub>; ASTM D1709/A |
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals |