Polymer Property : Dart Drop Test = 250 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 250 g
0.551 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene
Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h..
Dart Drop Test 250 g
0.551 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH..
Dart Drop Test 250 g
0.551 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a..
Dart Drop Test 250 g
0.551 lb
F50; ISO 7765-1
Polimeri Europa Clearflex® FG B0 Very Low Density Polyethylene
Clearflex FG B0 is a linear low density polyethylene, with antioxidants, suitable for blown film technology.Films made with Clearflex FG B0 are highly transparent, have good sealing properties, even..
Dart Drop Test 250 g
0.551 lb
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Dart Drop Test 250 g
0.551 lb
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Dart Drop Test 250 g
0.551 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a..
Dart Drop Test 250 g
0.551 lb
F50; ASTM D-1709
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,..
Dart Drop Test 250 g
0.551 lb
50µ; ISO 7765-1
Total Lacqtene® FB 3010 LDPE blown film  (discontinued **)
Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 180 to 220°C.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form..
Dart Drop Test 250 g
0.551 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim..
Dart Drop Test 250 g
0.551 lb
ASTM D1709
LG Chemical SEETEC EF221 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical Properties Additives: Antiblocking agent, Slip AgentApplications: Agricultural FilmCAS No. 24937-78-8Information provided by LG Chemical
Dart Drop Test 250 g
0.551 lb
ASTM D1709-98
Ipiranga Petrochem LB 0120 BPS LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Dart Drop Test 250 g
0.551 lb
ASTM D1709-98
Ipiranga Petrochem LBH 0117 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Dart Drop Test 250 g
0.551 lb
ASTM D1709-98
Ipiranga Petrochem LTH 0212 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..
Dart Drop Test 250 g
0.551 lb
Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height.
Kraton® D1102 + LDPE blend (2/98)
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Dart Drop Test 250 g
0.551 lb
ASTM D1709A
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..
Dart Drop Test 250 g
0.551 lb
ASTM D1709
ExxonMobil Pax-Plus™ 3208 Blown Film Resin
Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform..
Dart Drop Test 250 g
0.551 lb
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi..
Dart Drop Test 250 g
0.551 lb
ASTM D1709
Arkema Group OREVAC® 9318 EVA Terpolymer
OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre..
Dart Drop Test 250 g
0.551 lb
50 microns film
Arkema Group Orevac® 9318 Film EVA-MAH Terpolymer
EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group
Dart Drop Test 250 g
0.551 lb
ASTM D1709
Huntsman PE1451 EVA Film Extrusion  (discontinued **)
4.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..