Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 155 g | 0.342 lb | ASTM D1709 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |