Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 115 g | 0.254 lb | ASTM D1709 |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Dart Drop Test | 115 g | 0.254 lb | Method A; ASTM D1709 |
Dow 611A Low Density Polyethylene (LDPE) A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Dart Drop Test | 115 g | 0.254 lb | ASTM D1709 |
Huntsman PE1203 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |