Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 112 g | 0.247 lb | ASTM D1709 |
Dow DOWLEX™ 2038 Linear Low Density Polyethylene Linear Low Density PolyethyleneInformation provided by Dow |
|||
Dart Drop Test | 112 g | 0.247 lb | Method A; ASTM D1709 |
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene Fast processing on narrow die gaps For blown film paper product over wrap applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Dart Drop Test | 112 g | 0.247 lb | Method B; ASTM D1709 |
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe.. |