Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 560 g | 1.23 lb | 22; ASTM D 1709/A |
NOVA Chemicals Sclair® FP019-C Octene Copolymer LLDPE Film Resin FP019-C is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Polymer Process AidApplications: High toughness film,.. |
|||
Dart Drop Test | 560 g | 1.23 lb | 22; ASTM D 1709/A |
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig.. |