Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 425 g | 0.937 lb | (method A); ASTM D1709 |
Petroquimica Triunfo Tritheva® TN 8093 EVA Copolymer The Tritheva TN 8093 resin is a fractional MI copolymer of Ethylene-Vinyl Acetate (EVA), developed to meet the multi-layer and blending film applications where are required high strength, with high .. |
|||
Dart Drop Test | 425 g | 0.937 lb | ASTM-D1709 (Method B) |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |