Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 280 g | 0.617 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |
|||
Dart Drop Test | 280 g | 0.617 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Dart Drop Test | 280 g | 0.617 lb | F50; ISO 7765-1 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Dart Drop Test | 280 g | 0.617 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-317 EVA Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 5.5% vinyl acetate copolymer film resin. Film made from LD-317 offers excellent impact strength, tensile properties, and h.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709 |
Huntsman PE1501 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with excellent impact strength, good heat seal, and good clarity.Applications: Film extrusion: greenhouse film, heavy-duty packa.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709 |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Dart Drop Test | 280 g | 0.617 lb | ISO 7765-1 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709 |
ExxonMobil Enable™ 20-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 20-05CH is a metallocene ethylene-hexene copolymer. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and p.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709A |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709A |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709A |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Dart Drop Test | 280 g | 0.617 lb | ASTM D1709A |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |