Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 114 g | 0.251 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |