Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-108 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer high clarity film resin with a good balance of toughness, stiffness, and drawdown capability. This resin has good machinability in ba.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-306 EVA Film Resin, High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.5% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D882 |
Dow XU 66129.00 Developmental Monolayer Adhesive Film XU 66129.00 Developmental Monolayer Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-backed fabrics, paper, fiberglass, non-wovens, and rigid ure.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® HD-7000F HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7000F exhibit excellent impact and toughness properties as well as high stiffness.. |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Elmendorf Tear Strength, TD | 3.15 g/micron | 80.0 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |