Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 2.83 g/micron
72.0 g/mil
ASTM D1922
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo..