Polymer Property : Elmendorf Tear Strength, TD = 647.07 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene
Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene
Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by ..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have..
Elmendorf Tear Strength, TD 25.475 g/micron
647.07 g/mil
ISO 6383-2
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c..