Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
Eastman D4028-F Polyethylene  (discontinued **)
D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
Eastman E6838-014F Polyethylene  (discontinued **)
E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
ExxonMobil Escorene® LD-113 LDPE General Purpose Packaging Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin that offers a good balance of toughness, drawdown capability, stiffness and clarity. LD-113 exhibits good machinability in..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
ExxonMobil Escorene® CR-5810 EVA Resin, for High Cling Stretch Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A tackified Ethylene Vinyl Acetate resin for blown or cast stretch film.Applications: Packing films (cling). Data for film properties below based o..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
50 µm (2 mil) film; ASTM D1922
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion ..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ASTM D1922
ExxonMobil LD 141.87 Shrink Film Resin
LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade
DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an..
Elmendorf Tear Strength, TD 6.30 g/micron
160 g/mil
ISO 6383-2
Total LDPE 1022 FN 24 Low Density Polyethylene - Blown Film
LDPE 1022 FN 24 is a low density polyethylene made by a high pressure process without antioxidant.LDPE 1022 FN 24 is suited to many applications in the field of consumer, industrial, food or hygiene..