Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 6.20 g/micron | 157 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Elmendorf Tear Strength, TD | 6.20 g/micron | 157 g/mil | ASTM D-1922 |
Bapolene® 350F Polyethylene, Film Grade Applications: Blown film extrusion of T-shirt sacks, merchandise bags.Film properties below are based on a thickness of .8 mil and blow-up ratio of 4:1.Bapolene® and Bapolan® are registered tradem.. |
|||
Elmendorf Tear Strength, TD | 6.20 g/micron | 157 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films.. |