Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
SABIC HP0322N Low Density Polyethylene for Blown Film Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr.. |
|||
Elmendorf Tear Strength, TD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin
(discontinued **) Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at .. |
|||
Elmendorf Tear Strength, TD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANZEX® HF7700 High density polyethylene HF7700 is a high density polyethylene resin for tubular film extrusion. HF7700 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1.. |