Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, TD = 5.6045 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 5.6045 g/micron
142.35 g/mil
ISO 6383-2
Polimeri Europa Greenflex® FF 55 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 55 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 55 show high flexibility.Main Applications: Greenflex FF 55 is recommended f..
Elmendorf Tear Strength, TD 5.6045 g/micron
142.35 g/mil
ISO 6383-2
Polimeri Europa Riblene® FH 20 Low Density Polyethylene - Blown Film Extrusion
Riblene FH 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 20 is characterized by a good balance between processability and mechanical properties.Films manufac..
Elmendorf Tear Strength, TD 5.6045 g/micron
142.35 g/mil
ISO 6383-2
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m..
Elmendorf Tear Strength, TD 5.6045 g/micron
142.35 g/mil
ISO 6383-2
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit..
Elmendorf Tear Strength, TD 5.6045 g/micron
142.35 g/mil
ISO 6383-2
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe..