Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D 1922 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D 1922 |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin
(discontinued **) LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne.. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Elmendorf Tear Strength, TD | 18.0 g/micron | 457 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 13J7 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Film.Data provided by the manufacturer. |