Polymer Property : Elmendorf Tear Strength, TD = 437 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 17.2 g/micron
437 g/mil
ASTM D 1922
NOVA Chemicals Surpass® FPs016-C Octene sLLDPE Film Resin
FPs016-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem..
Elmendorf Tear Strength, TD 17.2 g/micron
437 g/mil
ASTM-D1922
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer
The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I..