Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 15.7 g/micron
399 g/mil
ASTM D1922
NOVA Chemicals Novapol® 20% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
Elmendorf Tear Strength, TD 15.7 g/micron
399 g/mil
ASTM D1922
NOVA Chemicals Novapol® 5% LF-0718-A in PF-0118-B LDPE Film Resin
Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical ..
Elmendorf Tear Strength, TD 15.7 g/micron
399 g/mil
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good..