Polymer Property : Elmendorf Tear Strength, TD = 3.50 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 3.50 g/micron
88.9 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin
Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da..
Elmendorf Tear Strength, TD 3.50 g/micron
88.9 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-Y819-A LDPE Film Resin
Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, shrink film, blends with LLDPE, small dia..
Elmendorf Tear Strength, TD 3.50 g/micron
88.9 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin
Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da..
Elmendorf Tear Strength, TD 3.50 g/micron
88.9 g/mil
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..