Polymer Property : Elmendorf Tear Strength, TD = 267 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 10.5 g/micron
267 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut..
Elmendorf Tear Strength, TD 10.5 g/micron
267 g/mil
ISO 6383-2
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene
Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire..