Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have.. |
|||
Elmendorf Tear Strength, TD | 25.475 g/micron | 647.07 g/mil | ISO 6383-2 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |