Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | ASTM D1922 |
Polymer Industries Densetec HDPE Rod Polymer Industries’ HDPE Rod exhibits all the durable qualities found in Densetec HDPE Sheet, making it perfect for that industrial application where sheet stock is not suitable. The HDPE Rod is av.. |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | |
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin 17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur.. |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 585 g/mil | ASTM D1922 |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | ASTM 1922 |
Braskem Flexus® 7200 LLDPE Cast Film Extrusion Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing.. |
|||
Elmendorf Tear Strength, TD | 23.0 g/micron | 584 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer. |