Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | >= 18.9 g/micron | >= 480 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, TD | >= 18.9 g/micron | >= 480 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, TD | 18.9 g/micron | 480 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin
(discontinued **) Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Elmendorf Tear Strength, TD | 18.9 g/micron | 480 g/mil | |
Westlake LF1021 Butene Linear Low Density Polyethylene Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant .. |