Polymer Property : Elmendorf Tear Strength, TD = 18.3 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 18.3 g/micron
465 g/mil
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and..