Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 16.9 g/micron | 429 g/mil | |
NOVA Chemicals Sclair® FPr017-D Octene LLDPE Film Resin FPr017-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPr0.. |
|||
Elmendorf Tear Strength, TD | 16.9 g/micron | 429 g/mil | ASTM D1922 |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Elmendorf Tear Strength, TD | 16.9 - 31.2 g/micron | 429 - 792 g/mil | Average value: 23.3 g/micron Grade Count:34 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |