Polymer Property : Elmendorf Tear Strength, TD = 16.5 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 16.5 g/micron
420 g/mil
ASTM D1922
ExxonMobil Exceed™ 1318CA Blown Film Resin  (discontinued **)
Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi..
Elmendorf Tear Strength, TD 16.5 g/micron
419 g/mil
ASTM D1922
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng..
Elmendorf Tear Strength, TD 16.5 g/micron
420 g/mil
ASTM D1922
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..