Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene
Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte..
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Riblene® FF 30 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 30 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 30 is characterized by a good melt strength leading to a good bubble stabilit..
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a ..
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s..
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion
Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit..
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion
Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p..
Copyright © lookpolymers.com All Rights Reserved