Polymer Property : Elmendorf Tear Strength, TD = 135 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 135 g/micron

@Thickness 0.0250 mm
3430 g/mil

@Thickness 0.000984 in
ASTM D1922
Equate EFDC-7087 LLDPE Film Extrusion Resin
EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-..