Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 0.512 g/micron | 13.0 g/mil | ASTM D1922 |
NatureWorks® Ingeo™ 4043D General Purpose Film Grade Biopolymer Ingeo 4043D can be converted into a biaxially oriented film with use temperatures up to 265ºF (130ºC). This film has excellent optics, good machinability and excellent twist and deadfold. These pr.. |
|||
Elmendorf Tear Strength, TD | 0.512 g/micron | 13.0 g/mil | Calculated from mfr's report of 1.8 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 419 Paper, 13 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Elmendorf Tear Strength, TD | 0.512 g/micron | 13.0 g/mil | Calculated from mfr's report of 1 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |