Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Elmendorf Tear Strength, TD | >= 12.0 g/micron | >= 305 g/mil | ASTM D1922 |
Eastman Eastar 5445 PCTG Copolyester, Film
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 14K1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, TD | 12.0 g/micron | 305 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-0242-E Hexene LLDPE Film Resin
(discontinued **) Excellent stiffness and glossApplications: Diaper back sheet, BlendingFilm properties are typical of film extruded at 270°C.Information provided by NOVA Chemicals. |
|||
Elmendorf Tear Strength, TD | 12.0 - 45.3 g/micron | 305 - 1150 g/mil | Average value: 27.2 g/micron Grade Count:64 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m.. |