Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion Riblene FF 22 is a high molecular weight low density polyethylene (LDPE), with added slip agent, suitable for blown film extrusion. Riblene FF 22 is characterized by a good melt strength leading to.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 20 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Films produced with Greenflex FD 20 exhibit good optical properties, high impact resistance, tensile .. |
|||
Elmendorf Tear Strength, TD | 4.076 g/micron | 103.5 g/mil | ISO 6383-2 |
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ.. |