Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
SABIC F00952 High Density Polyethylene for Blown Film Product Description: F00952 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
SABIC F00952EQ High Density Polyethylene for Blown Film Product Description: F00952EQ is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. the design of the product, molecular architect.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF260YZ Low density polyethylene LDF260YZ is a low density polyethylene resin for film extrusion. LDF260YZ has no slip and anti-block additives. LDF260YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact .. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF260GG Low density polyethylene LDF260GG is a low density polyethylene resin for film extrusion. LDF260GG has medium slip and anti-block additives. LDF260GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Elmendorf Tear Strength, TD | 4.02 g/micron | 102 g/mil | Calculated from mfr's report of 5.2 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Elmendorf Tear Strength, TD | 4.00 g/micron | 102 g/mil | ASTM-D1922 |
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR.. |