Polymer Property : Elmendorf Tear Strength, MD = 9.20 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 9.20 g/micron
234 g/mil
Dow DOWLEX™ 2071 Linear Low Density Polyethylene
DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks..
Elmendorf Tear Strength, MD 9.20 g/micron
234 g/mil
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a..
Elmendorf Tear Strength, MD 9.20 g/micron
234 g/mil
ASTM 1922
Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem
Elmendorf Tear Strength, MD 9.20 g/micron
234 g/mil
ASTM D1922
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..