Polymer Property : Elmendorf Tear Strength, MD = 8.82 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 8.82 g/micron
224 g/mil
ASTM D1922
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es..
Elmendorf Tear Strength, MD 8.82 g/micron
224 g/mil
ASTM D1922
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo..