Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 8.30 g/micron | 211 g/mil | |
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |