Polymer Property : Elmendorf Tear Strength, MD = 8.27 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 8.27 g/micron
210 g/mil
ASTM D1922
ExxonMobil Exceed™ 1012CA Film Resin  (discontinued **)
Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a..
Elmendorf Tear Strength, MD 8.27 g/micron
210 g/mil
ASTM D1922
ExxonMobil LD331.08 EVA LD 331.08 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical
Elmendorf Tear Strength, MD 8.27 g/micron
210 g/mil
ASTM D1922
ExxonMobil LD331.99 EVA LD 331.99 Very Clear, High Impact Film Resin
LD 331 Series films have superior impact strength and heat sealabilityInformation provided by ExxonMobil Chemical