Polymer Property : Elmendorf Tear Strength, MD = 70.0 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 2.76 g/micron
70.0 g/mil
ASTM D1922
ExxonMobil LL 1107x93 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Elmendorf Tear Strength, MD 2.76 g/micron
70.0 g/mil
ASTM D1922
ExxonMobil LL 1107x95 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..