Polymer Property : Elmendorf Tear Strength, MD = 7.776 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, MD 7.776 g/micron
197.5 g/mil
ASTM D1922
Dow DOWLEX™ 2083G Linear Low Density Polyethylene
Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow