Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
SABIC 518N Linear Low Density Polyethylene for Blown Film Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF200GG Low density polyethylene LDF200GG is a low density polyethylene resin for film extrusion. LDF200GG has medium slip and anti-block additives. LDF200GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF200YZ Low density polyethylene LDF200YZ is a low density polyethylene resin for film extrusion. LDF200YZ has no slip and anti-block additives. LDF200YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
Lotte Chemical Titan TITANLENE® LDF201FG Low density polyethylene LDF201FG is a low density polyethylene resin for film extrusion. LDF201FG has low slip and anti-block additives. LDF201FG meets the U.S. Food and Drug Administration (FDA) criteria for food contact .. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | |
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM-D1922 |
Braskem FC31D LLDPE Blown Film Extrusion Polyethylene Copolymer The FC31D resin is a linear low-density polyethylene, copolymer of butene -1, produced by the solution process for blow film extrusion. It has excellent mechanical properties, especially hot tack. I.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM-D1922 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM D1922 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |
|||
Elmendorf Tear Strength, MD | 6.00 g/micron | 152 g/mil | ASTM-D1922 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |