Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | >= 5.91 g/micron | >= 150 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4117N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | >= 5.91 g/micron | >= 150 g/mil | ASTM D1922 |
NIZHNEKAMSKNEFTEKHIM PE 4118N (18401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE. S.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock, Process Aid Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE. Slip 0 ppm. Antiblock.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922A |
LyondellBasell Montell 16501F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922A |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922A |
LyondellBasell Montell 16501F6 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets .. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922A |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922A |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Metabolix M-vera™ B5010 Film Grade Compostable Bioplastic For use in tough, certified compostable film and bag applications. Mvera B5010 offers a wide range of attractive traits—excellent tear and puncture toughness, excellent seal strength, good prin.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L42009H Film (Butene Grade) LLDPE Butene Copolymer (Barefoot/with high AO)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administr.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L42009B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Formosa Plastics Formolene® L42009E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyo.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation .. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Calculated from mfr's report of 10 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D882 |
Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | ASTM D1922 |
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industr.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Elmendorf Tear Strength, MD | 5.91 g/micron | 150 g/mil | Notched; ASTM D1922 |
Chevron Phillips 6109M LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |