Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, Medium Slip, Medium Antiblock Version of 7109TCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7109DT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, No Slip, No Antiblock Version of 7109T with Process Aid, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or ble.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips 7109T LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Blown Film at 1 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | Notched; ASTM D1922 |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | ASTM D1922 |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Elmendorf Tear Strength, MD | 16.5 g/micron | 420 g/mil | ASTM D1922 |
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste.. |