Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | ASTM D1922 |
NOVA Chemicals Novapol® TF-0219-E Hexene LLDPE Film Resin Exceptional toughens, Low gel levelApplications: Cast stretch wrapAdditives: High temperature A/OFilm properties are typical of cast film extruded at a melt temperature of 540°F, and a line speed o.. |
|||
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | ASTM D 1922 |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | ASTM D1922 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | ASTM D1922 |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Elmendorf Tear Strength, MD | 16.0 g/micron | 406 g/mil | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |